Unless stainless steel ties are specified, ACI (American Concrete Institute) recommends patching, partially filling or plugging the finished depression / holes left by form ties in the concrete surface. Why?




To prevent corrosion of the tie or staining of the concrete surface.
are-review.blogspot.com

Comments

Try These Too!

Heat gain calculation

Which lighting produces a 654.72 Btu/hr heat gain? A. 4x 40 watt fluorescent bulbs B. 2 x 75 watt incandescent C. 12 x 12 watt LEDs Answer (1 watt = 3.41 Btu/hr) A. 4x40 watts x 1.2 (for ballast) x 3.41 Btu/hr ARE 4.0 exam prep: BS

Bolted connections

What is the minimum spacing of bolts specified by AISC? and preferred spacing? A. 1 1/4 times the diameter of the bolt; 2 times preferred B. 1 3/4 times the diameter of the bolt; 2 1/4 times preferred C. 2 1/3 times the diameter of the bolt; 2 2/3 times preferred D. 2 2/3 times the diameter of the bolt; 3 times preferred E. 3 times the diameter of the bolt; 3.25 times preferred

Thermal insulation

Which of the following types of thermal insulation can be blown into wall or ceiling cavities with least difficulty, but contains no adhesive properties? I. Cellulose II. Rock wool III. Vermiculite IV. Mineral wool V. Straw VI. Polyicynene Answer I, II and III are loose-fill types of insulation that can be blown. IV comes in batts, V can come in boards or bales, VI is a spray-foam that adheres to the cavity. ARE 4.0 exam prep: BS